Products Description
The electrolyte used for testing is NCM electrolyte (KLD-1230C).
The range for compacting the electrode :
The electrode sheets are baked at 85°C for 4 hours, with a sealing pressure of 1300 psi.
Advantage: High-rate fast charging
Technical Parameters
D50 (um) | 9.0+-1.5 |
D10 (um) | 5.0+-2.0 |
BET (m2/g) | 1.40+-0.30 |
Tap density (g/cm3) | 1.05+-0.10 |
D90 (um) | 15.5+-3.0 |
Storage:
Appearance: Black powder, uniform color, free from agglomeration, and impurities.
Packaging requirements: Sealed with vacuum aluminum-plastic film, outer layer packaged in plastic bags.
Storage requirements: Sealed, stored in a cool, dry place.