Products Description
Materials need to be vacuum sealed for storage;
The electrolyte used during testing is: ternary electrolyte;
Baking conditions for electrodes are 85 ℃ for 4 hours, with a sealing pressure of 1300psi
Advantage:
- lithium cobalt oxide, single crystal structure, with small particle size and large specific surface area, facilitating rapid insertion and extraction of lithium ions, resulting in excellent rate performance and good cycling stability.
- Good processability and stable quality for commercial mass production.
- Widely used in high-rate requirement products such as drones and electronic cigarettes.
- Convenient for research on flexible packaging and button cells.
Technical Parameters
D10 (um) | 6.95 |
D50 (um) | 9.55 |
D90 (um) | 13.05 |
Specific surface area (m2/g) | 0.533 |
Vibration density (g/cm3) | 2.61 |
1ST Disch. (mAh/g) | 217.8 |
1ST Eff (%) | 90 |
Physical Property: High capacity, high Coulombic efficiency.
Storage:
Appearance: Black powder, uniform color, free from agglomeration, and impurities.
Packaging requirements: Sealed in vacuum aluminum-plastic film packaging, outer layer packed in plastic bags.
Storage requirements: Sealed, stored in a cool and dry place.