| Storage conditions |
| Keep sealed to avoid direct sunlight. Recommended storage temperature 20±10℃, humidity ≤50%RH. The shelf life is 1 year. If the product exceeds the shelf life, it should be inspected by our company and re-evaluated for normal use. |
| Under the condition of opening, strictly control the storage humidity ≤30%RH, and use as soon as possible. |
|
| Usage Suggestions |
| This product can be used as cathode electrode material in lithium ion secondary battery manufacturing. |
| The design capacity of the full battery with graphite anode: 163mAh/g (0.5C, 4.2V-3.0V). |
| Before batching, it is recommended to bake the materials at 120℃ for 6h. |
| Processing design compaction 3.20 ~ 3.40g/cm3. |